Test Item | Unit | Specification | ||||||
6μm | 7μm | 8μm | 9/10μm | 12μm | 15μm | 20μm | ||
Cu Content | % | ≥99.9 | ||||||
Area Weight | mg/10cm2 | 54±1 | 63±1.25 | 72±1.5 | 89±1.8 | 107±2.2 | 133±2.8 | 178±3.6 |
Tensile Strength(25℃) | Kg/mm2 | 28~35 | ||||||
Elongation(25℃) | % | 5~10 | 5~15 | 10~20 | ||||
Roughness(S-Side) | μm(Ra) | 0.1~0.4 | ||||||
Roughness(M-Side) | μm(Rz) | 0.8~2.0 | 0.6~2.0 | |||||
Width Tolerance | Mm | -0/+2 | ||||||
Length Tolerance | m | -0/+10 | ||||||
Pinhole | Pcs | None | ||||||
Change of Color | 130℃/10min 150℃/10min | None | ||||||
Wave or Wrinkle | ---- | Width≤40mm one allow | Width≤30mm one allow | |||||
Appearance | ---- | No drape, scratch, pollution, oxidation, discoloration and so on that effect using | ||||||
Winding method | ---- | The winding when facing up S sideWhen the winding tension in the stable, no loose roll phenomenon. |